Cement-Sand Plaster | JK GYPSUM Plaster | |
1 | Needs to be mixed in ratios controlled by labour | Only a single powder to be mixed with water, hence no ratios monitoring is required |
2 | Coarse finish - depends on sand fineness | Smooth finish with 200 mesh of fine gypsum. |
3 | Needs water curing twice a day for 8 - 10 days, million gallons of ground water is required for curing. Can go for Primary Painting After 72 Hours of GYPSUM Punning. Thus by Saving 35 to 40% of time in completion of the project. |
No water curing required, thus saving of million gallons of water and power |
4 | Time consumption is more for readying for painting | 25 to 30 % of time is saved |
5 | Needs putty or POP for bonding before painting | Single coat of putty with 1-2 mm thick is sufficient. |
6 | Prone to get cracks easily and naturally | Create anti-crack or no cracks will be developed on surface |
7 | The space looks smaller and unappealing as it is dark grey in color | The space looks large and beautiful as it is pure white in color |
8 | Cannot be applied on smooth surfaces | Can be applied on all masonry surfaces |
9 | Looks patchy in repair works and hairline cracks will develop | Excellent for repair works & can conceal with smooth finish without cracks |
10 | High density & more weight | Low density & low weight |
11 | Difficult and expensive for excellent finish. | Easy workability and economical |
12 | High Spoilage, more debris and garbage | No Spoilage and less debris |
13 | Underground water source is rapidly depleted due to excessive consumption of water for curing | No water is required, thus adhering to green building concept |
14 | No thermal properties | Having Thermal properties keeps cool 10 or 20 from outside Temperature |